Crystalline calcium silicate hydrate compounds: xonotlite (6CaO.6SiO2.H2O) and gyrolite (4CaO.6SiO2.3H2O) synthesized at CaO/SiO2 mole ratios of 0.67 and 1.0 under hydrothermal conditions show cation exchange capacities amounting to 41.70 and 44.40 meq/100 g respectively. They also exhibit cation exchange properties toward alkalimetal ions such as Na+and K+ as hydroxides (MOH) with concentrations ranging from 0.005-0.10 mol/l. The uptake of M+ by the gyrolite solid was found to be larger than xonotlite. It also increases with the increase of MOH concentrations and/or the time of reaction. This uptake was reached the equilibrium after 24 hrs, and the amount of K+-ions entered into the crystal structure of the solids (mmol/ 100 g) was found to be larger than Na+-ions. The equilibrium amounts of alkali-metal ions incorporated into the mentioned solids (mmol/100 g) were found to be 40.96 for K+ and 39.97 for Na+ with gyrolite, 37.44 for K+ and 36.74 for Na+ with xonotlite at 0.1 M MOH after 24 hrs. The Ca2+⇔M+ ratio (M+/Ca2+) was found to be 1 at concentrations up to 0.025 mol/l MOH with a slight decrease of a value smaller than 1 at higher concentrations. The affinities of xonotlite and gyrolite for alkali metal ions can be used for their separation from solutions. The mechanism of the exchange reaction is discussed.
No takes yet. Share an insight, caveat, or question.
Sabry A. El‐Korashy (2004) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: