Answers are grounded in this paper and cite their sources.
Device miniaturization requires dimensional shrinkage not only in the lateral directions but also in the vertical direction. A silicide contact in a shallow junction Si device has to be shallow, which means that in forming the silicide it may not consume more than a few hundred angstroms of Si from the substrate. A general scheme of making such a shallow silicide contact is reported here. The scheme utilizes the effect of alloying to dilute the contact reaction, and it produces a shallow contact and a protective diffusion barrier at the same time. Results of Pt-Cr alloys are presented for illustration.
No takes yet. Share an insight, caveat, or question.
Tu et al. (1980) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: