Answers are grounded in this paper and cite their sources.
Although ytterbium aluminum garnets (YbAG) belong to a group of promising optical materials, no physical method of thin films deposition has been described so far. In this work we present the comparison of two valuable physical deposition techniques: pulsed laser deposition and electron beam evaporation. Erbium (Er 3+ ) doped ytterbium garnet (Er 0.005 Yb 0.995 ) 3 Al 5 O 12 (Er:YbAG) thin films were prepared using own sol-gel derived ceramic targets. The phase composition of the films and crystallite size were determined using X-ray diffraction. Microstructure and surface morphology were studied by scanning electron microscopy and atomic force microscopy. Deposition parameters of used methods were optimized; however, both techniques produced amorphous films with insufficient microstructure. The effect of additional annealing on the crystallinity and luminescent properties of erbium ions was studied. A pure infrared emission of Er 3+ ions was observed only in samples prepared by pulsed laser deposition with subsequent annealing.
No takes yet. Share an insight, caveat, or question.
Tomáš Hlásek (2016) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: