Answers are grounded in this paper and cite their sources.
This study presents a low-temperature plasma-enhanced atomic layer deposition (PEALD) technique for fabricating high-performance, stress-reduced anti-reflective coatings (ARCs). To the best of our knowledge, this is the first extensive study on titanium dioxide (TiO2)/silicon dioxide (SiO2) stacking with PEALD at such a low temperature of 70 °C, which may help to overcome high-temperature deposition issues and mechanical stress for polymer substrates. Despite the presence of impurities in the low-temperature deposited films, the measured extinction coefficient (k < 10–4) indicates negligible optical absorption in both TiO2 and SiO2 layers, ensuring optimal performance for ARCs. Stress compensation is observed between tensile TiO2 films (≈ 220 MPa) and compressive SiO2 films (≈ − 35 MPa). For multi-layer ARCs, this combination strategy leads to a very low total stress of 48 MPa, which is a big step forward for stress control in optical coatings. This stress-reduction effect remains effective even when the thickness difference reaches up to 9.6%. This consistency has been demonstrated in real-world applications, where achieving an ideal level of thinness can be challenging. The optimized process at 150 W plasma power produces high-quality optics with an average reflectivity of 0.35% in the visible range while maintaining low stress, a significant achievement in low temperature deposited optical coatings. The choice of common, cost-effective materials like SiO2 and TiO2 makes this approach easily scalable for industrial use and can see the future of manufacturing ARCs for various applications. These films are characterized by a low density of defects and an amorphous structure with the smoothness of their surface being close to one atomic monolayer (≈ 0.2 nm), which indicates their high optical quality, comparable to films deposited at high temperatures. The low-temperature PEALD presented in this work not only pushes the boundary in advanced optical coatings but also enlarges the capacity in coating temperature-sensitive substrates and complex 3D structures. This innovation paves the way for applications in bendable electronics, high-performance optical components, and next generation display devices.
No takes yet. Share an insight, caveat, or question.
Cu et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: