We present a systematic reliability study of PZT polarization retention after exposure to high temperatures and high-field cycling. After a 260 °C Pb-free solder assembly reflow-like exposure, a signal margin of >10 μC/cm 2 is achieved at a read voltage of 1 V. Extraction of the Preisach distribution after thermal depolarization and restore exhibits an increase in the positive coercive voltage by 45 % while the negative coercive voltage shows minimal deviation (<;7 %). Under accelerated aging via high electric fields (2.4 V), maximum wake-up at 10 6 cycles followed by fatigue >10 8 cycles is observed. Asymmetry in coercive voltage is minimized after wakeup and remanent polarization maximized. After fatigue, a signal margin >10 μC/cm 2 is maintained for read voltages >0.8 V.