Answers are grounded in this paper and cite their sources.
Experimental evaluation demonstrates the tribological performance of LTB and LTBGr alloys, suggesting optimal compositions for wear resistance.
: In the submersible, HSC (half split casing), and end suction centrifugal pump sets, sand cast LTB (leaded tin bronze) alloys are well-liked bearing alloys. The comparative tribological characteristics of LTB and LTBGr are shown by this experimental investigation. The presence of α and δ phases in the copper matrix is determined by the quantity of Sn element in the composition, according to morphological analysis of sand-cast mixed LTB alloys using an optical emission microscope (OEM). Up to 9% of Sn by weight, solid solution α-phase formation was observed; nucleation for ẞ and δ phase formation occurred after this, which is converted into δ phase at room temp.. The addition of Sn% increases the hardness of LTB alloys, while the increase in Pb% acts as a softening agent between 3.5 and 14.5% of Sn; however, after 12% of Sn addition, third-body abrasion due to brittleness and pullout character increases in the wear of LTB alloy. The highest wear resistance was found as 2.86x10‾4 mg/ Nm and COF of 0.560 at 1500 rpm and 50 N normal load,10 minutes rotation for Cu 9Sn10Pb2Ni1Zn alloy, while optimum wear resistance and optimum COF of values 2.76x10‾3mgN/m and 0.34 for Cu 10 Sn11Pb 2Ni 1Zn. Similarly, the optimum wear resistance and COF values were found as3.00x10‾3 mg/Nm and 0.207 at the same testing parameters for Cu 10Sn 8Pb 2Ni 1Zn 2Gr.
No takes yet. Share an insight, caveat, or question.
Chauhan et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: