Demonstrates recovery of uniform elongation in cold-rolled pure Ni after hydrogen charging, indicating potential for improved material performance.
Uniform elongation of severely cold-rolled metallic materials is generally poor. For example, cold-rolled pure Ni with a 93% thickness reduction exhibits necking immediately after yielding. This study demonstrates that the uniform elongation of severely cold-rolled pure Ni recovers after charging with 100 MPa hydrogen gas (hydrogen concentration: 49.5 mass ppm). Specifically, hydrogen charging increased the uniform elongation of the cold-rolled pure Ni plate from approximately 0.4% to 2.5% at a strain rate of 10 −3 s −1 . The extent of uniform elongation recovery increased with increasing strain rate. In addition, the deformation behavior of the hydrogen-charged cold-rolled Ni fully reverted to that of the uncharged material after aging in air at 200°C for 114 h, during which hydrogen was completely desorbed.
No takes yet. Share an insight, caveat, or question.
Koyama et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: