Answers are grounded in this paper and cite their sources.
Randomized trial evaluates how restoration design affects fracture resistance in teeth with lesions, suggesting ways to improve dental repair.
PURPOSE: To evaluate the effect of different preparation designs and ceramic thicknesses on the fracture resistance and failure mode of maxillary premolars with non-carious cervical lesions restored with milled lithium disilicate laminate veneers. MATERIALS AND METHODS: Seventy-eight sound maxillary premolars were randomly assigned to six groups (n = 13) based on preparation design and thickness: BC3 (0.3 mm buccal reduction), BR3 (same as BC3 with composite resin restoration filling the lesion), BRO3 (same as BR3 and 1 mm occlusal reduction for buccal cusp slopes), BC5, BR5, and BRO5; prepared as contralateral groups but with buccal reduction of 0.5 mm. All specimens were restored with lithium disilicate laminate veneers, subjected to 10,000 thermocycles and 240,000 chewing cycles (49 N), and then loaded to failure at a 45° angle. Data were analyzed using two-way ANOVA and chi-square tests (α = 0.05). RESULTS: There was a significant main effect of preparation design on fracture resistance (p < 0.001), whereas ceramic thickness (p = 0.470) and the interaction between design and thickness (p = 0.138) did not reach statistical significance. Moreover, there was a significant difference in the failure mode between tested groups (p < 0.001) with predominant Type II unrepairable failure in the ceramic material, leaving the tooth intact for BRO groups. CONCLUSIONS: All tested designs provided mean fracture resistance values within the physiological bite force range for all tested groups for the premolar region, this must be interpreted alongside the failure mode distribution. BC and BR preparation designs demonstrated a clinically meaningful rate of catastrophic Type IV root fractures, whereas BRO preparations produced predominant cohesive ceramic failure Type II. The thickness of the lithium disilicate laminate veneers, whether 0.3 or 0.5 mm, did not significantly affect fracture resistance or failure patterns.
No takes yet. Share an insight, caveat, or question.
Abdelnaby et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: