Answers are grounded in this paper and cite their sources.
Examines diffusion bonding performance in high entropy alloy and steel, suggesting optimal conditions for bonding strength and ductility.
Diffusion bonding of reduced-activation Cr 0.8 FeMn 1.3 Ni 1.3 high entropy alloy (HEA) to F82H is often limited by insufficient interfacial atomic transport. Here, a dislocation-assisted strategy is employed by introducing controlled pre-deformation in the HEA prior to spark plasma sintering diffusion bonding. EBSD-based GND analyses confirm that increasing the cold-rolling reduction from 20 % to 30 % enhances dislocation storage and promotes short-circuit diffusion, leading to a pronounced broadening of the interdiffusion zone from 18.28 μm to 25.8 μm. In contrast, extending the pre-annealing time at 20 % reduction mainly accelerates recovery and stimulates extensive Cr-rich BCC precipitation within grain interiors, while providing only a marginal increase in interdiffusion distance. The 30 % reduction condition produces a distinct interfacial state characterized by a wider diffusion zone, smoother compositional gradients, and predominantly grain-boundary-confined precipitation, resulting in an optimized strength-ductility balance with UTS of 461 MPa and elongation of 13.52 %. These findings demonstrate that joint performance is governed by a defect-state window in which dislocation-enabled diffusion is maximized.
No takes yet. Share an insight, caveat, or question.
Xue et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: