Demonstrates effective copper recovery from low-grade sulfide concentrates, indicating a robust recovery solution.
The accumulation of low-grade, refractory copper sulfide concentrates from secondary resources, such as smelting slag-flotation products, represents a growing challenge in the copper industry. This study develops and validates an atmospheric oxygen-enriched leaching process that requires neither grinding nor high pressure, targeting a typical slag-flotation copper sulfide concentrate. Systematic mineralogical analysis shows that copper is 95% in secondary sulfides, with quartz, chlorite, and muscovite as major gangue. Batch leaching optimization identifies the following conditions: H2SO4 250 g/L, temperature 90 °C, leaching time 8–12 h, pulp density 30–33% solids, and oxygen-enriched air (80–90% O2) at a flow rate ensuring sufficient oxygen mass transfer. Under these conditions, copper extraction reaches 97–99% without grinding. Continuous pilot-scale trials (over 500 kg dry feed) compare a five-stage mechanically agitated tank train and a four-stage tower reactor. The tank train achieves a stable copper extraction of 97.1% with a residue grade of 0.53% Cu at 8 h residence time and acid consumption of 857 kg/t concentrate, significantly outperforming the tower reactor. Reducing oxygen purity from 100% to 90% has no measurable effect on extraction, while 80% O2 gives only a 2% loss. The process eliminates grinding, operates at ambient pressure, and uses widely available reactor technology, offering a potentially low-capital and technically robust solution for recovering copper from such refractory secondary sulfide concentrates.
No takes yet. Share an insight, caveat, or question.
Zhou et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: