Evaluates erosion mechanisms in stainless steel, suggesting new indicators of damage progression.
Cavitation erosion has an incubation stage during which the surface degrades without measurable mass loss. Gravimetric methods miss this entirely. To get around the problem, we used relocation SEM combined with Fourier-based power spectral density (PSD) analysis on SUS 304 stainless steel. The cavitation test followed ASTM G32. Exposure was applied in 5 min steps up to 45 min. After every step, the same surface regions were re-imaged. SEM images were taken at four magnifications: 2500×, 5000×, 7000×, and 15000×. PSD analysis gave us two parameters: the slope β and the intercept C. Both were measured across several non-overlapping subregions to improve the reliability of the statistics. β increased at all magnifications, indicating roughening from cyclic plastic deformation, slip bands, and early microcracks. At 2500×, β went from 2.62 (polished surface) to 3.91 at 40 min, with R2 = 0.98. At 45 min the trend broke, which we interpret as the start of the acceleration stage. At this point, localized material detachment begins, partially smoothing the surface at certain length scales. β also strongly correlated with Ra, Rrms, and Rmax. But unlike those parameters, it carries multi-scale information about the damage. SEM images show that fatigue from repeated deformation is the main mechanism during incubation. Pits caused by individual microjets are rare and contribute little. Together, β and C serve as a sensitive indicator of the transition from incubation to acceleration and provide information that mass loss alone cannot.
No takes yet. Share an insight, caveat, or question.
Osman et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: