• We innovatively combined high-temperature calcination and acid leaching to reduce the amount of industrial solid waste coal gangue. • Two kinds of inorganic chemical products were prepared from coal gangue: acidic solution enriched with Al and Fe; A solid material rich in Si. • Through FT-IR, XRD, SEM and BET characterization analysis, the mechanism of mineral phase transformation and structure change before and after coal gangue treatment was elaborated in detail. • The removal rates of aluminum and iron are 90.84% and 97.68%, respectively. The proportion of silicon in silicon rich solid materials (SiO2) is as high as 83.90%. • It provides a new solution for the comprehensive utilization and sustainable utilization of coal gangue. The classification and extraction of valuable components from coal gangue is a way to improve the comprehensive utilization of coal gangue. However, the stable structure of kaolinite in coal gangue makes silicon and aluminum closely combined in minerals, which is difficult to separate by simple physical or chemical methods, and hinders its hierarchical extraction. In this study, a method of calcination activation acid leaching combined with reduction treatment of coal gangue was developed, and an aluminum iron enriched acidic solution and a silicon enriched material were prepared. The activation effect and mechanism of calcined coal gangue and the conversion mechanism of acid leaching extraction of metal aluminum were systematically studied. The results showed that the optimal calcination activation acid leaching process parameters were as follows: calcination temperature: 600 ℃, calcination time: 4 h, acid leaching time: 2 h, solid–liquid ratio of activated coal gangue and hydrochloric acid solution (g:ml): 1:12. After calcination under the optimal conditions, the layered structure of Kaolinite was destroyed and some layered silicate minerals, Berlinite (AlPO 4 ), FeS, which were soluble in hydrochloric acid solution, were formed. These minerals are dissolved in hydrochloric acid solution and then separated by solid–liquid separation after reaction. An acidic solution rich in aluminum and iron and a material rich in silicon were prepared, which made the recovery of Al and Fe reach 90.84 % and 97.68 %, respectively. And the enrichment rate of Si (SiO 2 ) reached 83.90 %.This provides a new solution for the comprehensive utilization and sustainable utilization of coal gangue.
No takes yet. Share an insight, caveat, or question.
Zhang et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: