Answers are grounded in this paper and cite their sources.
Treatment of the filler surface with a silane dressing agent, ensuring the chemical interaction on the filler–binder interface, and ultrasonic treatment of the compound enhance the physicomechanical properties of the epoxy composite: The failure stress and bending elastic modulus increase by a factor of 2–3. Considerable (2.5- fold) increase in the impact resilience even at 50% filling should be particularly noted. Introduction of modified brick dust enhances the heat resistance and thermal conductivity of the epoxy composite.
No takes yet. Share an insight, caveat, or question.
Мостовой et al. (2017) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: