This study explores how various fabrication parameters impact the thermal, rheological, and mechanical properties of composite filaments fabricated with reinforcement of secondary (2°) recycled polylactic acid (PLA) with waste wood dust (WD) using a mechanical blending technique. The filaments were produced by adjusting the temperature, torque, and load of a twin-screw extruder for use in applications of three-dimensional (3D) printing. This study demonstrates that melt flow index of filament reduces with an increase in the reinforcement percentage beyond certain limits. In this study, twin-screw extrusion has been used to prepare feedstock filament by reinforcing WD with 6 wt.% to impart required thermal, mechanical, and morphological properties. It has been examined that thermal, mechanical, and morphological properties of 2° PLA reinforced with 6 % by weight of WD exhibits superior peak strength (PS), low porosity percentage, and better thermal stability as compared with other filaments fabricated at different weight percentages on the basis of extrusion parameters. Optimal parameter setting that exhibits maximum PS (31.81 MPa), percentage elongation at break (%BE) (8.86 %) at 7.5-kg load, 175°C temperature, 0.1-Nm torque and 7.5-kg load, 185°C temperature, 0.2-Nm torque, respectively. This study not only emphasizes the impact of fabrication parameters on filament properties but also highlights the sustainable manufacturing aspect of using 2° PLA and WD as reinforcements. By incorporating recycled and waste materials, this approach contributes to reducing plastic waste and promoting sustainable and environmentally responsible manufacturing practices.
No takes yet. Share an insight, caveat, or question.
Kumar et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: