Answers are grounded in this paper and cite their sources.
The viscoelastic properties of a 4% solution of monodisperse polystyrene (molecular weight 394,000) in Aroclor 1260 were determined by the following techniques: creep recovery, stress relaxation upon cessation of steady flow, dynamic measurements, and normal stress difference and shear stress measurements in steady flow. All measurements were carried out with cone and plate geometry in a Weissenberg rheogoniometer. The modification of this instrument to perform creep and creep recovery experiments by use of an air‐bearing suspension and an air‐turbine drive is described. A broad range of shear rates and frequencies encompassing both linear and nonlinear behavior was employed. The elastic behavior is described in terms of the recoverable shear strain s or the steady‐state compliance J e °. The first three techniques gave identical results for J e ° in the range of linear viscoelasticity for which it is defined. The normal stress difference measurements confirmed Lodge's relation s = ( P 11 − P 22 )/2σ 21 . Reasons for previous experimental disagreement with this result are discussed.
No takes yet. Share an insight, caveat, or question.
Stratton et al. (1971) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: