Formulation of strain hardening cementitious composites typically engage 2% or more fiber by volume, resulting in higher cost and difficult processing. This study presents the development of strain hardening magnesium-silicate-hydrate composite with an extremely low fiber volume fraction of 0.5% via micromechanics-guided design approach. The developed composite demonstrated a tensile strain capacity of 7.2% with a tensile strength of 2.24 MPa, and a compressive strength of 86.1 MPa. The fiber/matrix interfacial bond was characterized using single fiber pullout test . The microstructural characterization of fiber surface and fiber tunnel in the matrix was carried out to understand the fiber/matrix interface properties . The micromechanics-based assessment of critical fiber volume fraction required to achieve strain hardening was also conducted. The material sustainability of the developed composite was evaluated and compared with existing Portland cement-based strain hardening cementitious composites , and strategies to further reduce embodied carbon and primary energy were proposed.
No takes yet. Share an insight, caveat, or question.
Sonat et al. (2023) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: