Answers are grounded in this paper and cite their sources.
Explores optical properties of CdSxSe1-x films in optoelectronics, indicating compositional control is possible.
This work explores a chemical bath deposition (CBD) route to fabricate cadmium sulfide-selenide (CdS x Se 1-x ) solid solution films with tunable composition and properties for optoelectronics. Theoretical calculations of the boundary conditions for the CdS and CdSe formation in the citrate-ammonia-thiourea-selenosulfate system were made. The boundary conditions of CdS x Se 1-x were defined by the overlap area between the constructed CdS and CdSe formation zones. Single-phase CdS x Se 1-x films were successfully deposited at a cadmium salt concentration of 0.005 mol/L and a thiourea concentration of 0.05 mol/L, with sodium selenosulfate concentrations varying from 0.001 to 0.025 mol/L, corresponding to (NH 2 ) 2 CS: Na 2 SeSO 3 molar ratios of 50 : 1, 20 : 1, 10 : 1, 5 : 1, and 2 : 1, as confirmed by XRD analysis. This resulted in a substitutional parameter x ranging from 0.30 to 0.84, as determined by XRF. The optical and morphological properties of CdS x Se 1-x films were investigated. Optical transmittance measurements revealed a bandgap variation from 1.94 to 2.52 eV. The films exhibited continuous surface coverage, with morphology strongly dependent on Na 2 SeSO 3 concentration and deposition time. These findings demonstrate that controlled CBD enables precise tuning of composition and optical properties, providing a platform for potential optoelectronic applications.
No takes yet. Share an insight, caveat, or question.
Guminilovych et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: