Answers are grounded in this paper and cite their sources.
Silicon wafer was bonded to stainless steel substrate by a silver-containing silicate binder. The bond was subjected to thermomechanical fatigue with temperature variation from 20 to 900 °C. The bond showed an initial shear strength of 8.2 MPa. The thermomechanical aging caused progressive decrease in shear strength. After the first three cycles of fatigue, the shear strength dropped to 5.15 MPa. The shear strength was 3.2 ± 0.54 MPa after 5 cycles of thermal cycling. The shear strength further decreases to 1.35 MPa after 10 cycles of thermal aging. The modulus of rigidity or shear modulus of the initially bonded joint was measured as 1.5 ± 0.18 GPa. After 5 thermomechanical cycles, the modulus of rigidity dropped to 0.84 ± 0.07 GPa. After 10 cycles, the modulus of rigidity dropped to 0.49 ± 0.11 GPa. The ductility of the bond is very limited (less than 1.3% before cycling tests). After thermomechanical cycling, the bonded joints showed the ductility in the range from 0.38% to 0.63%, indicating the embrittlement of the joint under the thermomechanical fatigue conditions. AC impedance measurement on the bond revealed transition from resistive to capacitive after thermomechanical cycling. Interfacial debonding is the dominant mechanism for thermomechanical fatigue failure, but fracture of the adhesive was also observed. Pore formation in the adhesive layer was revealed by fracture surface morphology analysis.
No takes yet. Share an insight, caveat, or question.
Gan et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: