The thermal resistivity, Seebeck coefficient, electrical resistivity, and Hall mobility of Ge-Si alloys have been measured throughout the Ge-Si alloy system as functions of impurity concentration in the range 2×1018−4×1020cm−3, and of temperature in the range 300°–1300°K. A qualitative interpretation of these properties is given. For power conversion, boron and phosphorus were found to be useful p-type and n-type impurities, respectively, because of their high solid solubilities. At 1200°K, the maximum values of the dimensionless figure of merit zT were 0.8 for p-type Ge0.15-Si0.85 alloy doped to 2.1×1020cm−3 holes, and 1.0 for n-type Ge0.15-Si0.85 alloy doped to 2.7×1020cm−3 electrons. The maximum over-all efficiency of a stable generator operating between 300°–1200°K, using the best p-type and n-type materials was computed to be 10%.
No takes yet. Share an insight, caveat, or question.
Dismukes et al. (1964) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: