This study applies the accumulative roll bonding (ARB) technique is used to produce ultra–fine grained Al–Cu–Ag shape memory alloys. Pure Al (aluminium), Cu (copper) sheets, and Ag (silver) particles were used as primary materials. The aluminium content was fixed at 11 wt.% in all composites, while silver was varied at 1, 2.5, and 5 wt.%. After accumulative roll bonding (ARB) processing, the layered composites were annealed between 800°C and 1100°C for one hour and then quenched to the room temperature. The effects of Ag (silver) concentration and heat treatment temperature on microstructure were examined as the novelty of this work. All samples exhibited refined grains and high dislocation density. Heat treatment process generated new intermetallic phases. For alloys with 1 wt.% Ag, the dominant phase was Cu9Al4. Increasing Ag value up to 2.5–5 wt.% stabilised orthorhombic Cu3Al martensite. Formation of martensite enhanced strength and microhardness at the ambient conditions. The highest martensite fraction was obtained at 900°C–1000°C. Annealed and quenched composites showed excellent shape memory behaviour at the ambient temperature. These findings show that ARB offers a promising alternative route for producing ultrafine–grained Cu–based SMAs with enhanced martensite stability and shape–memory performance.
No takes yet. Share an insight, caveat, or question.
Yang et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: