Answers are grounded in this paper and cite their sources.
A novel electrode geometry and contacting procedure has allowed measurement of the quasi-Fermi levels, i.e., apparent electrochemical potentials, of electrons and holes at an illuminated semiconductor / liquid contact. key feature of our experiments is the use of a lithographically patterned, high purity (100-400 Ω-km n-type zone material), low dopant density Si sample in contact with CH_3OH-dimethylferrocene^(+/o) solutions. photogenerated carriers can be collected at the back side of the Si sample through a series of diffused n+ p^+ points. The lifetime of photogenerated carriers approaches 2 ms in this sample, indicating that electronhole is minimized in the bulk of the semiconductor. Furthermore, surface recombination is by use of low saturation current density, ohmic-selective contacts at the back of the sample. The /liquid contact also has a low recombination rate. Therefore, the potentials measured at the diffused points values for the quasi-Fermi levels of electrons and holes under illumination of the semiconductor/ liquid . Transient photovoltage measurements have also been performed to confirm quantitatively that the quasi-Fermi levels are flat across the Si samples used in this work.
No takes yet. Share an insight, caveat, or question.
Tan et al. (1994) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: