Answers are grounded in this paper and cite their sources.
Strong green and red visible emissions were obtained from ZrO2:Yb3+–Er3+ nanocrystals synthesized by sol-gel method and annealed at 1000 °C for 5 h. The average crystallite size was ∼70 nm with tetragonal phase for total concentration lower than 3 mol % and cubic phase for concentration higher than 5 mol %. The color coordinate of the upconverted signal was tailored by controlling the dopant composition that change the red/green ratio dominated by the cross relaxation and energy back transfer process as was demonstrated theoretically and confirmed experimentally. Both coefficients were calculated, C51∼1.02×10−16 and C5b∼6.04×10−17, from the theoretical model based on the rate equations. The highest energy transfer efficiency was η∼64% for 2 mol % of Yb and 2 mol % of Er3+. However, for the highest upconverted signal was only η∼29% obtained for 2 mol % Yb and 1 mol % Er with effective decay time τeff∼438 μs for red and τeff∼290 μs for green band.
No takes yet. Share an insight, caveat, or question.
Solís et al. (2010) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: