This is the authors' abstract. We don't add key points for this paper.
Most of the high-strength aluminium alloys for Laser Powder Bed Fusion (L-PBF) in research are based on conventional hardenable Al–Cu, Al–Mg–Si and Al–Zn–Mg alloys that have issues with hot-cracking during the L-PBF process. This study investigates the effect of alloying elements on two novel Al–Cr–Mo-Sc-Zr alloys (Scancromal® variants) with a good, crack-free processability and strength-ductility combination. A layer thickness of 100 μm was used, highlighting the high productivity and good processability of Al–Cr alloys. Heat treatments and hardness measurements were conducted to investigate peak age heat treatment and revealed a relation between Sc/Zr-ratio and peak aged temperature. SEM observations of small precipitates at grain boundaries and fracture surfaces contributed to understanding the changing fracture mechanism from less ductile (2.4–10.2% elongation) to very ductile (14.1–19% elongation). Tensile tests at elevated temperatures and creep tests showed a positive effect of Cr and Mo on high temperature strength . High-temperature properties, especially creep results of Al–Cr alloys and Scalmalloy® (Al–Mg–Mn-Sc-Zr) are presented for the first time and emphasize the increased heat-resistance by Cr and Mo. The threshold stress, below which theoretically no creep should occur, of the presented Scancromal® variants is at least 5 times higher (142–189 MPa) compared to Scalmalloy® (28 MPa). A comprehensive comparison of the results to literature values of AlSi10Mg, other Al–Cr alloys and high temperature Al alloys gives valuable insight on how the aging response, microstructure, ductility and high-temperature strength of this type of alloy is influenced by its alloying elements.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Agricola et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: