Answers are grounded in this paper and cite their sources.
In the current study, elevated heat resistance of the mortars including 15% fly ash, ground granulated blast furnace slag and silica fume is investigated. Fly ash, ground granulated blast furnace slag and silica fume are replaced with cement past by weight in the prepared mortar samples. The prepared samples are kept in a furnace for 2 hours at 400 °C and 800 °C to find out effect of elevated temperature on compressive strength of the mortars. Compressive strength before and after heat exposure are measured in terms of evaluating elevated heat resistance. Control sample that does not contain any admixture, mortar including fly ash, mortar including ground granulated blast furnace slag and mortar including silica fume has 30.81 MPa, 33.62 MPa, 43.91 MPa and 51.83 MPa compressive strength before heat exposure, respectively. Compressive strength of the same samples after 400 °C and 800 °C heat exposure are 25.64 MPa and 8.12 MPa, 28.91 MPa and 11.56 MPa, 34.37 MPa and 15.21 MPa and 39.78 MPa and 21.85 MPa, respectively. The alteration of heat resistance of the mortars with fly ash, ground granulated blast furnace slag and silica fume is attributed to puzzoulanic behavior of the used materials. These materials react with Ca(OH)2 in cement and produce extra tobermorite gel (CSH phase) that provides extra durability to the composite.
No takes yet. Share an insight, caveat, or question.
Murat Öztürk (2022) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: