Transmission and reflection data (0.5-5 eV) for 300 AA PdH x thin films (x=0.65, 0.85 and 0.92), hydrogenated under high-pressure conditions are presented and compared with similar data for pure palladium before and after hydrogen desorption. The main difference in transmission data consists of a pronounced peak around 1 eV in the transmission of PdH x compared with the structureless continuously increasing transmission in pure palladium. This confirms the theoretical expectation of Khan and Riedinger (1982) that the inter-band absorption edge in PdH occurs at about 1 eV. The reflectivity data were measurable for PdH 0.65 only; samples with higher hydrogen contents (x=0.85 and x=0.92) exhibit a reflectivity below 0.5%, which is thus not quantitatively measurable by the method applied. This high reduction in the reflectivity cannot be explained by the increase in surface roughness only. A possible contribution from hydrogen itself is briefly discussed.
No takes yet. Share an insight, caveat, or question.
Wyrzykowski et al. (1989) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: