This paper describes a study on the effects of <TEX>Mg₂Si₍ₚ₎</TEX> addition on the microstructure, porosity, and mechanical properties namely hardness and tensile properties of AA332 composite. Each composite respectively contains 5, 10, 15, and 20 wt% reinforcement particles developed by a stir-casting. The molten composite was stirred at 600 rpm and melted at <TEX>900∘C±5∘C</TEX>. The <TEX>Mg₂Si</TEX> particles were wrapped in an aluminum foil to keep them from burning when melting. The findings revealed that the microstructure of <TEX>Mg₂Si₍ₚ₎/AA332</TEX> consists of <TEX>α</TEX>-Al, binary eutectic (<TEX>Al+Mg₂Si</TEX>), <TEX>Mg₂Si</TEX> particles, and intermetallic compound. The intermetallic compound was identified as Fe-rich and Cu-rich, formed as polygonal or blocky, Chinese script, needle-like, and polyhendrons or "skeleton like". The porosity of <TEX>Mg₂Si₍ₚ₎/AA332</TEX> composite increased from 8-10% and the density decreased from 9-12% from as-cast. Mechanical properties such as hardness increased for over 42% from as-cast and the highest UTS, elongation, and maximum Q.I were achieved in the sample of 10% <TEX>Mg₂Si</TEX>. The study concludes that combined with AA332, the amount of 10 wt% of<TEX>Mg₂Si</TEX> is a suitable reinforcement quantity with the combination ofAA332.
No takes yet. Share an insight, caveat, or question.
Zainon et al. (2016) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: