As part of a comprehensive study of the copolymer system poly(ethylene terephthalate‐sebacate), specific heat measurements have been carried out on the annealed polyester, poly(ethylene sebacate), over the temperature range −20 to 140°C. From estimates of densities of completely crystalline and amorphous polymer, the crystallinity at room temperature was calculated to be 57%, and the heat of fusion of completely crystalline polymer to be 30.5 cal. g. −1 , a value considerably greater than that calculated by Edgar and Ellery from copolymer data. This discrepancy is attributed to the small crystallite size in their copolymer study. It is shown that the low melting point of the aliphatic polyesters as compared to that of polyethylene is due to the low heat of fusion rather than to a large entropy of fusion as previously supposed. Finally, it is pointed out that in the liquid range, the heat content is closely proportional to volume.
No takes yet. Share an insight, caveat, or question.
Wunderlich et al. (1958) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: