Epitaxial thin films of orthorhombic KNbO 3 (100)/(010) were deposited on MgO (100) single‐crystal substrates by pulsed laser ablation using an ε120 Å SrTiO 3 (110) transition layer in between. From X‐ray diffraction, the orientation relationships were determined as (010) [100] or (100) [010] KNb0 3 ∥ (110) [110] SrTiO 3 ∥ (100) [011] MgO and (010) [001] or (100) [001] KNbO 3 ∥ (110) [001] SrTiO 3 ∥ (100) [011] MgO. The measured film refractive indices at 632.8 nm were 2.213 ± 0.003, 2.278 ± 0.003, and 2.285 ± 0.003, respectively, along MgO [100], [011], and [011] directions. A model was developed to correlate the measured effective refractive indices of the film to area fractions of domain variants in the film. Using the model, the area fraction of domains with their polarization axis normal to the substrate was estimated to be 60.0 ± 2.7%.
No takes yet. Share an insight, caveat, or question.
Gopalan et al. (1995) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: