The catalytic activity for methylcyclohexane dehydrogenation was compared for Pt particles on four different oxide supports (SiO 2 , Al 2 O 3 , TiO 2 , and ZrO 2 ). At reaction temperatures of 220 °C and 300 °C, the Pt/Al 2 O 3 catalyst had the best long-term stability and conversion, while the Pt/SiO 2 catalyst deactivated the most rapidly. Temperature programmed oxidation experiments on the post-reaction Pt/SiO 2 and Pt/TiO 2 catalysts at 220 °C demonstrated that a large fraction of carbonaceous species resides on Pt, and therefore deactivation is attributed to the blocking of the metallic sites. In contrast, for Pt/Al 2 O 3 and Pt/ZrO 2 , the stable activity at 220 °C is explained by migration of carbonaceous residues to the support. In general, the extent of catalyst deactivation increases with increasing deposition of carbonaceous residues on the Pt sites; these CH x species are characterized as soft coke that can be removed by hydrogenation at 300 °C. Ammonia temperature programmed desorption experiments indicated that catalyst deactivation decreases with increasing number and strength of acidic sites. The acidic sites on the support are proposed to decompose CH x species that migrate from the particle to the support so that the Pt surface can be kept free of foulants. Pt/TiO 2 catalysts that were heated in H 2 at 600 °C to induce Pt decoration by TiO x exhibited excellent long-term stability, which is attributed to the loss of the larger Pt ensembles necessary for coking.
No takes yet. Share an insight, caveat, or question.
Tengco et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: