This is the authors' abstract. We don't add key points for this paper.
The oxidation behaviour of two single crystal Ni-based superalloys has been investigated at 450°C and 550°C. Isothermal oxidation was carried out for varying times and it was found that exposure resulted in a sub-micrometre thick oxide. The external and internal oxide kinetics were studied via high-resolution image analysis and both showed sub-parabolic growth rates. Thermogravimetric tests indicated that the overall oxidation growth obeys a near quartic power law while parabolic kinetics can describe the transient oxidation period. Characterisation of the resulting oxides was carried out using electron microscopy, energy dispersive spectroscopy and X-ray diffraction. Results from thermodynamic modelling of the oxide formation are also presented to further assess the postulated mechanism of low-temperature oxidation in these Ni-based superalloys.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Evangelou et al. (2018) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: