Answers are grounded in this paper and cite their sources.
Both InP and InxGa1−xAsyP1−y surfaces with trace metal contaminations are unstable with respect to cone formation when sputter etched by Ar+. Such gross surface texture severely degrades the depth resolution of sputter profiling techniques. Cone formation can be prevented by avoiding contamination of the material being profiled with metals sputtered from various surfaces in the analysis system. An uncorrected width of 140 Å was determined using techniques which optimize sputter depth profiling for an In0.74Ga0.26As0.60P0.40-InP heterojunction grown by liquid phase epitaxy.
No takes yet. Share an insight, caveat, or question.
Williams et al. (1980) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: