Answers are grounded in this paper and cite their sources.
We have studied the glass transition in vitreous silica using the technique of high-temperature light scattering. We report the temperature dependence of the Landau-Placzek ratio of Homosil up to and through the glass transition. The results show that the compressibility {β} of silica increases sharply at Tg with {β}(T>Tg)/{β}(TTg){}3.8. In contrast to the results of Bucaro and Dardy, our data show the expected sharp change in slope for the Landau-Placzek ratio as a function of temperature at Tg, and no anomalous behavior is observed below that temperature. The relaxation of the Landau-Placzek ratio at high temperature has also been studied and is compared with the annealing behavior of the Raman defect lines (490 and 605 cm^-1) at the same temperatures. The average relaxation time {τ}{} for RLP is {}(2--3)×{}10⁵ s at 1000 ^∘{}C and {}10⁴ s at 1100 ^∘{}C, in good agreement with the relaxation times derived from viscosity data. For the Raman lines, {τ}{} is found to be much smaller (10⁴ s at 1000 ^∘{}C) indicating that different structural rearrangements are responsible for the two relaxation processes.
No takes yet. Share an insight, caveat, or question.
Krol et al. (1986) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: