Raman spectra of two superionic conducting crystals, fcc Li₂{SO}₄$ and bcc ${LiAgSO}₄$, have been recorded in the frequency range 300--1400 ${cm}^{{{-}}1}$ across the entire temperature range of stability of each compound. Comparison of polarized and depolarized spectral bandwidths for the symmetric ${A}₁$ sulfate internal mode permits a component due to the sulfate-ion reorientation to be separated, which confirms the plastic behavior of the superionic phases of the two crystals. In the case of ${Li}₂SO₄, the reorientation time derived corresponds well with the value 2 ps recently reported on the basis of computer-simulation studies. Our measurements are precise enough to yield the temperature dependence of the reorientation time in each type of crystal. The Arrhenius activation energies are significantly different: 0.40 and 0.72 eV for fcc Li₂{SO}₄$ and bcc ${LiAgSO}₄$, respectively. These values are sufficiently close to the contrasting activation energies for cation diffusion, 0.34 and 0.52 eV, respectively, to support the ``paddle-wheel'' migration postulate for this type of plastic crystal.
No takes yet. Share an insight, caveat, or question.
Börjesson et al. (1985) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: