A wavelength dependent, quantitative comparison of the static magneto-optical signal in Co-Pt and Co-Pd alloys, Co/Pt and Co/Pd multilayers and TbFeCo has been carried out. Dynamic testing of evaporated Co-Pt and Co-Pd alloys, embedded in quadrilayer structures has been demonstrated at 488nm. Large mark CNR ratios above 60dB in Co-Pt alloys were found on ungrooved glass disks.