Answers are grounded in this paper and cite their sources.
Thermodynamic parameters (work W def and heat Q def) of inelastic deformation (uniaxial compression up to ɛdef = 50%) are measured for six samples of high-molecular-mass linear PE at room temperature under the regime of active loading. Energy excess ΔU def accumulated by the samples subjected to loading are calculated in terms of the first law of thermodynamics. All thermodynamic characteristics linearly increase with crystallinity χ of PE, thus making it possible to extrapolate their values to χ = 0 and 100% and to find the contributions of the amorphous and crystalline phases of the polymer to the overall thermodynamics of deformation. Both of the PE phases contribute to W def and ΔU def, while the crystalline phase alone contributes to heat Q def. At ɛ ≥ 30%, the energy contribution from the amorphous phase exceeds that from the crystalline phase. A comparison between the plastic behavior of PE crystals and glassy polymers demonstrates that PE crystallites are easier deformed (requires less work W def) than glassy polymers. At the same time, the amorphous phase of PE is harder to deform (requires more work W def and stores more energy ΔU def) than noncrystalline rubbers, apparently because of the deformation of tie chains. The thermodynamic characteristics of deformation are compared for three materials: crystalline metals, PE, and glassy polymers. The similarities and differences in their plastic behaviors are considered.
No takes yet. Share an insight, caveat, or question.
Salamatina et al. (2011) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: