Answers are grounded in this paper and cite their sources.
We report controlled hole expansion in photonic crystal fibres (PCFs) by heating the fibre while the holes were pressurised. This was done by post-processing an existing fibre, not during fibre fabrication. Small holes in an endlessly single-mode (ESM) PCF were inflated to become large holes. The large-hole PCF was then tapered to produce a "cobweb" PCF with a small highly-nonlinear core, interfaced to the ESM PCF at both ends by gradual transitions. The loss was less than 0.4 dB in the complete structure, which was used to demonstrate supercontinuum generation when pumped with a fs Ti:sapphire laser.
No takes yet. Share an insight, caveat, or question.
Wadsworth et al. (2005) studied this question.