In this study, we developed a high-performance low-temperature polycrystalline silicon thin-film transistor (LTPS-TFT) incorporating an ultra thin Eu2O3 gate dielectric. High-κ Eu2O3 LTPS-TFT annealed at 500 °C exhibits a low threshold voltage of 0.16 V, a high effective carrier mobility of 44 cm2/V-s, a small subthreshold swing of 142 mV/decade, and a high Ion/Ioff current ratio of 1.34 × 107. These significant improvements are attributed to the high gate-capacitance density due to the adequate quality of Eu2O3 gate dielectric with small interfacial layer of effective oxide thickness of 2.5 nm. Furthermore, the degradation mechanism of positive bias temperature instability was studied for a high-k Eu2O3 LTPS-TFT device.