Answers are grounded in this paper and cite their sources.
We have fabricated Mach–Zhender interferometers (MZIs) using the (Ba,Sr)TiO 3 (BST) film sputter-deposited at 450 °C, which is a critical temperature for the process after metallization. An optical modulation of about 10% is achieved when 200 V is applied (electric field in BST is 1.2 × 10 4 V/cm). However, the response time of optical modulation to step function voltage is slow (1.0–6.3 s). We propose a model for the slow transient behavior based on movable ions and a long dielectric relaxation time for the BST film, and good qualitative agreement is obtained with experimental results.
No takes yet. Share an insight, caveat, or question.
Suzuki et al. (2007) studied this question.