The microwave losses in both pure and doped SrTiO₃ have been investigated as a function of frequency and temperature. It is found that the loss tangent is proportional to frequency in the range 3-36 kMc/sec. Above the phase transition at 112^∘{}K, the temperature dependence of the loss tangent is well represented by tanδ=(T-Tc)^-1(α+βT+γT²), where the Curie temperature, Tc=37^∘K. The parameter α is shown to be determined by lattice imperfections and vanishes for pure single-crystalline material. The parameters β and γ, which are related to third-and fourth-order anharmonic terms in the interionic potential, are shown to be intrinsic properties of the perfect lattice and are unaffected by imperfections.