Answers are grounded in this paper and cite their sources.
Thin smooth anatase TiO 2 films are obtained by electron beam evaporation of reduced TiO 2 . These films show a preferential (004) orientation when deposited on electron beam evaporated amorphous titanium. Electrochemical lithium insertion into these films is studied with several optical and electrochemical techniques. A coloration efficiency of 13 cm 2 C -1 is found, which is twice as high as that reported for TiO 2 films grown by chemical vapor deposition (CVD). Potential-dependent capacitance measurements show that after the extraction of lithium ions has taken place a small region at the surface of the electrode has a much higher dielectric constant than that of the bulk of the electrode. This is explained by the presence of irreversibly trapped lithium ions in the region where a (reversible) phase transformation from anatase TiO 2 to anatase Li 0.5 TiO 2 has occurred. The extent of this region depends strongly on the intercalation potential; values of 7 and 17 nm are found after 2.5 h of intercalation at −1.0 and −1.2 V vs SCE, respectively. The dielectric constant of the modified surface region is found to range between 500 and 900. A scheme is proposed that describes the mechanism of lithium insertion in terms of a moving TiO 2 |Li 0.5 TiO 2 phase front.
No takes yet. Share an insight, caveat, or question.
Krol et al. (1999) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: