The thermal oxidation of Si with a planar interface in the dry oxidation condition is studied by constructing a continuum model based on a reparametrization-invariant reaction–diffusion equation. By analyzing the simulation results, it is found that the growth of the oxide thickness xo follows a time-dependent power law, xo ∼ (t/τ)ν, with the temporal exponent given by \(ν = 2- 1 + (5(1 + √2t/τ ))- 1\), where t denotes the oxidation time and τ [= 1 (h)] is a constant. The validity of this property is confirmed by comparing the evolution curves of xo according to the power law given above with the experimental data on the thermal oxidation of Si(100) in both dry and wet oxidation conditions and also those of SiC\((0001̄)\) C-face, SiC\((112̄0)\) a-face, and SiC(0001) Si-face in the dry oxidation condition. The implication of our results to the self-limiting oxidation of a Si nano wire is discussed additionally.
No takes yet. Share an insight, caveat, or question.
Makoto Itoh (2020) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: