The long-term integrity of wellbore sealants is critical for successful CO 2 storage in geological reservoirs. This paper addresses the durability of a one-part, granite-based geopolymer (GP) sealant batch-exposed to CO 2 and H 2 O, with or without H 2 S or H 2 SO 4 for up to 16 weeks. Microstructural and mineralogical changes were then characterized using a wide range of analytical techniques. Results show that exposure led to an increase in the material’s crystalline content. Vaterite was the dominant early carbonate in all cases. This then transformed primarily into aragonite in samples exposed to clean CO 2 , while calcite was more prominent in samples exposed to CO 2 with H 2 S or H 2 SO 4 . The matrix's crystallinity was further enhanced through consecutive reactions of aluminosilicate gels. Even though exposure resulted in elevated sulfur contents, no sulfur-bearing minerals were detected. Despite these alterations, the GP maintained its integrity during exposure to chemically aggressive conditions, demonstrating its durability as a sealant.
No takes yet. Share an insight, caveat, or question.
Hajiabadi et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: