Coercive force, remanence and maximum energy product of compacts of iron are measured as functions of density of packing ( d/d 0 ) and X-ray particle size ( L ). The iron is prepared by hydrogen reduction of ferric oxide and for the grade used optimum technical properties are: B r = 5200 gauss, ( B. H ) max = 0.82 × 10 6 gauss: oersted, and B H C = 400 oersted when L = 300 Å and d/d 0 = 0.5. Maximum coercive force obtained is 610 oersted when d/d 0 = 0.3. For d/d 0 fixed the three magnetic quantities increase with decreasing particle size, the increase being greatest with B r and ( B. H ) max . The increase in remanence is discussed in terms of its ratio to saturation magnetization and it is suggested that the observed increase is related to packing effects. Measurement of the influence of oxygen impurity indicates that the presence of a few per cent of oxide does not appreciably affect the quality of the magnets.
No takes yet. Share an insight, caveat, or question.
E H Carman (1955) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: