Spin reorientation of Nd2Fe14B with different degree of grain sizes was detected by measuring the temperature dependence of the ac susceptibility. The studied materials include: (1) a spherical Nd2Fe14B single crystal that shows no coercivity. (2) Microcrystalline Nd2Fe14B obtained by induction-melting or by sintering: Due to the presence of random-oriented multi-domain grains (⩾5000 nm), the bulk ingot shows no coercivity, but sintered materials do. (3) Microcrystalline Nd2Fe14B produced by the hydrogenation-disproportionation-desorption-recombination (HDDR): The HDDR treated materials show a coercivity due to the presence of single-domain grains of a size of about 200–300 nm. (4) Nanocrystalline Nd2Fe14B prepared by mechanical alloying and by rapid quenching: Due to the presence of ultrafine Nd2Fe14B grains (<50 nm), these materials show a high coercivity and an enhanced remanence. For the first time, a decrease of the spin-reorientation temperature, an intrinsic magnetic property, with decreasing the Nd2Fe14B grain size is found. The decrease of the spin-reorientation temperature in nanocrystalline Nd2Fe14B can be ascribed to the strong inter-grain exchange change coupling among nanocrystalline Nd2Fe14B.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Kou et al. (1997) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: