The evolution of the microstructure during heat treatment was investigated for dip-coated Bi/sub 2/Sr/sub 2/CaCu/sub 2/O/sub y/(Bi-2212)/Ag and Ag alloy tapes as a function of temperature and oxygen partial pressure (P(O/sub 2/)=0.01, 0.21 and 1 atm) using quenched and fully-processed tapes. The microstructures were essentially the same for Bi-2212 on pure Ag and on the Ag alloy, Although the melting temperature of Bi-2212 increased with increasing P(O/sub 2/), the solidification temperature (T/sub sol/) of Bi-2212 for P(O/sub 2/)=0.21 atm was higher than that for P(O/sub 2/)=1 atm. The volume fraction and grain alignment of Bi-2212 processed in P(O/sub 2/)=0.01 atm was smaller than in tapes processed in 0.21 and 1 atm, which were quite similar. HR-TEM studies on grain boundaries and AC susceptibility measurements suggest that the higher critical current density(J/sub c/) for tapes processed in P(O/sub 2/)=1 atm than that for 0.21 atm is due to improved coupling of the grains.
No takes yet. Share an insight, caveat, or question.
Fujii et al. (1997) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: