The behavior of dielectric and microwave properties against sintering temperature was been carried out on CaO-B 2 O 3 -SiO 2 glass-ceramics with Na 2 O addition by XRD and SEM. The results show that 0.5 wt.% Na 2 O addition is advantageous to improve the dielectric and microwave properties due to increasing the major crystalline CaSiO 3 . With further increasing Na 2 O content, α-SiO 2 is the predominant crystalline phase instead of CaSiO 3 . The CBS glass-ceramics with 0.5 wt.% Na 2 O sintered at 875°C has a bulk density of 2.51g·cm -3 , and which possesses good dielectric properties: ε r =6.2, tanδ =1.9×10 -3 (10 MHz) and low dielectric constant below 2×10 -3 over a wide frequency range. The proposed dielectrics can find applications in microwave devices, which require low dielectric loss and low dielectric constant.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Peng Wei (2013) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: