Answers are grounded in this paper and cite their sources.
Shows improved electrochemical performance in solid-state lithium-metal batteries, indicating better battery stability.
Sulfide-based solid-state electrolytes (SSEs) with high Li+ conductivity ( σ_Li⁺ ) and trifling grain boundaries have great potential for all-solid-state lithium-metal batteries (ASSLMBs). Nonetheless, the in-situ development of mixed ionic-electronic conducting solid-electrolyte interphase (SEI) at sulfide electrolyte/Li-metal anode interface induces uneven Li electrodeposition, which causes Li-dendrites and void formation, significantly severely deteriorating ASSLMBs. Herein, we propose a dual anionic, e.g., F and N, doping strategy to Li7P3S11, tuning its composition in conjunction with the chemistry of SEI. Therefore, novel Li6.58P2.76N0.03S10.12F0.05 glass-ceramic electrolyte (Li7P3S11-5LiF-3Li3N-gce) achieved superior ionic (4.33 mS·cm−1) and lowest electronic conductivity of 4.33 × 10−10 S·cm−1 and thus, offered superior critical current density of 0.90 mA·cm−2 (2.5 times > Li7P3S11) at room temperature (RT). Notably, Li//Li cell with Li6.58P2.76N0.03S10.12F0.05-gce cycled stably over 1000 and 600 h at 0.2 and 0.3 mA·cm−2 credited to robust and highly conductive SEI (in-situ) enriched with LiF and Li3N species. Li3N’s wettability renders SEI to be highly Li+ conductive, ensures an intimate interfacial contact, blocks reductive reactions, prevents Li-dendrites and facilitates fast Li+ kinetics. Consequently, LiNi0.8Co0.15Al0.05O2 (NCA)/Li6.58P2.76N0.03S10.12F0.05-gce/Li cell exhibited an outstanding first reversible capacity of 200.8/240.1 mAh·g−1 with 83.67% Coulombic efficiency, retained 85.11% of its original reversible capacity at 0.3 mA·cm−2 over 165 cycles at RT.
No takes yet. Share an insight, caveat, or question.
Fan et al. (2024) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: