Answers are grounded in this paper and cite their sources.
SnO2-CuO composite nanorods with a Janus structure were prepared by one-step flame spray pyrolysis. High-aspect-ratio SnO2 nanorods were positioned on one side of the spherical CuO powder. The mean length of the rod-shaped crystals decreased from 200 to 20 nm when the SnO2 content in the composite powders decreased from 70 to 10 wt%. Initially, SnO2-CuO composite nanopowders formed from the vapors in the high-temperature diffusion flame by surface growth and coagulation. Phase separation of the composite nanopowders occurred and rod-like Janus structures evolved during the growth of SnO2 and CuO crystals in the quenching process. The maximum charge capacities of pure SnO2 and the composite powders with SnO2/CuO of 90/10, 70/30, and 50/50 were 547, 499, 493, and 316 mA h g(-1), respectively, at a high current density of 3000 mA g(-1). The corresponding capacity retentions after 50 cycles were found to be 39, 47, 80, and 85%, respectively. The decrease in the charge capacity with increasing current density was slower in SnO2-CuO (70/30) composite powders than in pure SnO2. The Janus-structured SnO2-CuO (70/30) composite powders showed a high charge capacity and excellent cycling performance at high current densities.
No takes yet. Share an insight, caveat, or question.
Choi et al. (2013) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: