Attachment of four oligomeric (MW 550) ethylene glycol chains to tetraphenylporphyrin results in a highly viscous, room temperature melt a hybrid redox polyether that is highly concentrated in porphyrin sites (∼0.4 M) and will dissolve LiClO 4 electrolyte. Microelectrode voltammetry in undiluted, free base and Co and Fe-metalated melts yields apparent diffusion coefficients that for 1.2 M LiClO 4 electrolyte vary by >10 3 -fold, from a high of 6.2 × 10 -9 cm 2 s -1 for the ring reduction of the free base to a low of ca. 3 × 10 -12 cm 2 s -1 for the Co(II/III) oxidation in a Co-metalated melt. Taking the latter as measuring the true physical self-diffusivity of the porphyrins, electron self-exchange rate constants are found for four porphyrinic redox couples (free base (0/1−), Co(II/I), Fe(II/I), and Fe(III/II) give 3.6 × 10 6, 1.2 × 10 5, 3.7 × 10 4, and 1.1 × 10 4 M -1 s -1, respectively). An activation study yields large free energy activation barriers for these couples, and exponential pre-factors in the 10 13 −10 14 s -1 range. The polyether appendages provide a weakly coordinating “solvent” for the porphyrin centers, and the introduction of ligands like pyridine and carbon monoxide at the gas/melt interface causes changes in Fe(III/II) voltammetry consistent with axial coordination in the semisolid melt. The axial coordination and voltammetric change is reversed by removing the ligand from the bathing gas.
No takes yet. Share an insight, caveat, or question.
Long et al. (1997) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: