The scattering function was determined for four samples of atactic oligo- and poly(α-methylstyrene)s (a-PαMS), each with the fraction of racemic diads f r = 0.72, in the range of weight-average molecular weight M w from 1.27 × 10 3 to 6.46 × 10 4 in cyclohexane at 30.5 °C (ϑ) in the range of the magnitude k of the scattering vector smaller than 1 Å -1 by the use of a point-focusing small-angle X-ray scattering (SAXS) camera. The Kratky function F s as a function of k increases monotonically with increasing k for M w ≲ 5 × 10 3 and exhibits a plateau in the range of 0.15 Å -1 ≲ k ≲ 0.3 Å -1 for M w ≳ 5 × 10 3 . For k ≲ 0.5 Å -1, all the experimental data may be well explained by the corresponding helical wormlike (HW) chain theory. For k ≳ 0.5 Å -1, however, agreement between theory and experiment is only qualitative. A comparison is made of the present SAXS data for a-PαMS with the previous data for atactic polystyrene with f r = 0.59, atactic poly(methyl methacrylate) (a-PMMA) with f r = 0.79, isotactic PMMA with f r ≃ 0.01, and syndiotactic (s-) PMMA with f r = 0.92. It is then found that the HW theory may give a good explanation of the difference in the behavior of F s for k ≲ 0.3 Å -1 between the four polymers except s-PMMA, for which the HW model parameters have not been determined.
No takes yet. Share an insight, caveat, or question.
Ohgaru et al. (2000) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: